- 01 High stripping force, excellent adhesion;
- 02 Reduce contact resistance;
- 03 Good coating leveling;
- 04 Reduce polarization and improve magnification performance;
- 05 Protect fluid collection, improve cycle performance and extend battery life.
Aluminum foil after pretreatment (oil removal, corona).
It is suitable for printing and coating of imported or domestic gravure printing press, the speed is 60m-120m per minute.
peculiarity |
Standard |
Test method |
Coating appearance |
black |
Visual inspection |
PH value |
3-5 |
Automatic titrator |
Viscosity (cps) |
600-900. |
Rotary viscometer |
Solid inclusion |
15 + / - 1 |
Constant temperature drying oven 150℃/30min |
Coating color |
Grayish black to black |
Visual observation |
Levelling property |
Uniform no penetration |
KPP color observation |
Adhesive force |
No shedding |
3M600 tape strip |
Resistance (mΩ) |
1-3 |
Pole plate resistance meter |
Coating surface tension N/m |
60dyn |
Corona pen |
NMP |
200 times no aluminum leakage |
Cotton swab |
electrolyte |
200 times no aluminum leakage |
Cotton swab |
name |
index |
unit |
Coating technology |
Gravure coating |
- |
Applicable substrate |
Aluminum foil for lithium battery |
- |
preconditioning |
Oil removal/corona removal |
38 dynes above |
Plate temperature |
77-132. |
℃ |
Optimum engine speed |
60-120. |
m/min |
When using the paste, please do not miscible with other brands of paste, to avoid other abnormalities in the product;
Adjust diluents in different proportions according to requirements;
Before use, please mix with diluent and stir well to ensure consistency of product performance.